MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound RE0039 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP STAT-KON RE0039 compound is based on Nylon 6/6 resin containing 15% carbon fiber. Added features of this grade include: Electrically Conductive, Flame Retardant.

Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.550 %0.550 %23°C/50% RH/24 hrs; ASTM D570
 0.870 %0.870 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0017 - 0.0026 cm/cm0.0017 - 0.0026 in/in24hrs; ISO 294
 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0068 - 0.0078 cm/cm0.0068 - 0.0078 in/in24hrs; ISO 294
 0.0070 - 0.0080 cm/cm0.0070 - 0.0080 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 205 MPa29700 psiASTM D638
 209 MPa30300 psiISO 527
Elongation at Break 2.2 %2.2 %ASTM D638
 2.2 %2.2 %ISO 527
Tensile Modulus 15.6 GPa2260 ksi1 mm/min; ISO 527
 17.58 GPa2550 ksi50 mm/min; ASTM D638
Flexural Strength 297 MPa43100 psiASTM D790
 318 MPa46100 psiISO 178
Flexural Modulus 11.44 GPa1659 ksiASTM D790
 14.2 GPa2060 ksiISO 178
Izod Impact Notched 74.0 J54.6 ft-lbASTM D256
Izod Impact, Unnotched 7.04 J/cm13.2 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 46.0 kJ/m²21.9 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J5.90 ft-lbpeak; ASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  45.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 45.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
25.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 66.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 228 °C442 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 247 °C
@Thickness 3.20 mm
477 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 95.0 - 110 °C203 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81357 / 289304

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.