MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Algoflon® L100 PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® L100 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles.

Algoflon® L100 can be de-agglomerated to sub-micron particle size by the application of shear providing a better dispersion and distribution of the PTFE particles in the application.

Designed for use in critical engineering and high end performance lubricants, Algoflon® L100 will improved thickening effect, lubricity, improved corrosion and temperature resistance.

Main Algoflon® L100 features are:
- Low coefficient of friction and reduced wear
- Outstanding chemical and corrosion resistance
- High temperature resistance
- Good low temperature torque

Applications: Additive

Processing
- Algoflon® L100 micronized powder are ideal for dispersing in oils, greases and pastes to improve both high and low temperature lubricity and are preferred over conventional additives, such as graphite or molybdenum disulfide whenever potential staining cannot be tolerated.

- Greases incorporating up to 30% by weight of Algoflon® L100 micronized powder are effective for much longer periods than conventional greases so that lubrication frequency may be reduced substantially. Extreme environmental demands on greases, such as those experienced in the automotive industry (i.e. wide temperature ranges and heavy loads) can be accommodated by the addition of Algoflon® L100 micronized powders.

Storage and Handling
- Algoflon® L The usual precautions for safe storage and handling of Algoflon® L100 should be taken according to material safety documentation and experience. There will be no chemical deterioration of the Algoflon® L100 during proper storage.

- Shelf life of Algoflon® L100 micronized powders will vary depending upon whether the recommended storage conditions are maintained and whether the material remains free from foreign contamination during storage time (not exposed to dirt, dust, water or other chemicals). The material should remain sealed in the original containers and storage conditions should provide for protection from temperature extremes as well as rain, snow or other wet environments (or such conditions which may damage the storage containers in which the product is stored).

Safety and Toxicology
- Before using PTFE Algoflon® L100 micronized powders consult the product Material Safety Data Sheet and follow all label directions and handling precautions.

- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes. See Material Safety Data Sheet for detailed advice on waste disposal methods.

Packaging
- Algoflon® L100 is packaged in 15 kg non returnable drums. Each drum has one bag liner made of polyethylene resin.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.325 g/ccASTM D4894
Particle Size 20 µmAverage
Specific Surface Area >= 20 m²/g
 
Thermal PropertiesOriginal ValueComments
Melting Point 320 - 330 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorWhite
FormsPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4031 / 279831

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.