MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

MOL Group TIPELIN 6000B HDPE, Blow molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Description: TIPELIN 6000B is a high density bimodal polyethylene copolymer (with butene-1 as comonomer) intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR). The grade contains antioxidant and acid scavenger.

Applications: TIPELIN 6000B is recommended for thin walled, small bottles up to 5 liter capacity for consumer goods such as cosmetics, daily care etc. and for blow molded products for packaging of aggressive industrial chemicals bounded to UN certificates. It is suitable for corrugated pipes too.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291).

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³1; ISO 1183-1
ESCR 10% Igepal® 200 hour200 hour1, CO-630; ASTM D 1693
Oxidative Induction Time (OIT) 30 min
@Temperature 200 °C
30 min
@Temperature 392 °F
EN 728
Melt Flow  0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 1.3 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.3 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65651; ISO 868
Tensile Strength at Break 31.0 MPa4500 psi1; ISO 527-3
Tensile Strength, Yield 31.0 MPa4500 psi1; ISO 527-3
Elongation at Break 1200 %1200 %1; ISO 527-3
Elongation at Yield 10 %10 %1; ISO 527-3
Flexural Modulus 1.65 GPa239 ksi1; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²1; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 129 °C264 °F1; ISO 306/A 120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG035 / 297201

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.