ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries. ForTii® WX11-FC has excellent hydrolysis resistance, processability and surface quality and is ideal for complex and thin walled food and water contact applications. Features: USP class VI classified. Drinking Water Grade. 30% glass reinforced. Processing: Injection molding. Former DSM Engineering Plastics product line is now with Envalior. |