MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin NHP6012 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL NHP6012 resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a CTI 2 and UL94 flame rating of V0 at 1.5mm for thin-wall molding capability. NORYL NHP6012 is based on a unique co-polymer technology and exhibits high flow, high heat resistance, dimensional stability, hydrolytic stability, strong electrical performance, low moisture absorption and very low specific gravity. This material is an excellent candidate for appliance internals, indoor and outdoor electrical and electrical vehicle (EV) battery modules/housings.

Features: Strong Electrical Performance,Low Specific Gravity,Low Moisture Absorption,Hydrolytic Stability,High Heat Resistance,Good dimensional stability,Non-Chlorinated,Non-Brominated,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccISO 1183
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
 0.10 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0200 %23°C/50% RH/24 hrs; ISO 62-4
 0.0200 %Injection Molding
Moisture Absorption at Equilibrium 0.050 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 0.20 %ASTM D570
 0.20 %ISO 62-1
Viscosity 20 cP
@Load 10.0 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
 90ISO 2039-2
Ball Indentation Hardness 214 MPaH358/30; ISO 2039-1
Tensile Strength at Break 82.0 MPa5 mm/min; ASTM D638
 82.0 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ASTM D638
 2.5 %5 mm/min; ISO 527
Tensile Modulus 4200 MPa5 mm/min; ASTM D638
 4400 MPa1 mm/min; ISO 527
Flexural Strength 132 MPa1.3 mm/min, 50 mm span; ASTM D790
 132 MPa2 mm/min; ISO 178
Flexural Modulus 4000 MPa1.3 mm/min, 50 mm span; ASTM D790
 4000 MPa2 mm/min; ISO 178
Izod Impact Notched 70.0 JASTM D256
 60.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 440 J/mASTM D4812
 425 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1U
 25.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 25.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 25.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 3.00 Jpeak; ASTM D3763
 4.00 JASTM D3763
Dart Drop Test 136680 gASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.01e+16 ohm-cmASTM D257
 2.01e+16 ohm-cmIEC 60093
Surface Resistance 5.32e+15 ohmASTM D257
 5.32e+15 ohmROA; IEC 60093
Dielectric Constant 2.83
@Frequency 1e+6 Hz
ASTM D150
 2.83
@Frequency 1e+6 Hz
IEC 60250
 3.37
@Frequency 50.0 - 60.0 Hz
ASTM D150
 3.37
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 15.3 kV/mm
@Thickness 3.20 mm
in air; IEC 60243-1
 21.7 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 24.8 kV/mm
@Thickness 1.60 mm
in air; IEC 60243-1
 51.7 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0029
@Frequency 1e+6 Hz
ASTM D150
 0.0029
@Frequency 1e+6 Hz
IEC 60250
 0.1089
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.1089
@Frequency 50.0 - 60.0 Hz
IEC 60250
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 VIEC 60112
 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.00 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 33.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 58.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 58.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.210 W/m-KASTM D5930
 0.210 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 132 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 134 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 136 °CRate B/50; ASTM D1525
 136 °CRate B/50; ISO 306
 138 °CRate B/120; ASTM D1525
 138 °CRate B/120; ISO 306
 144 °CRate A/50; ASTM D1525
 144 °CRate A/50; ISO 306
UL RTI, Electrical 50.0 °CUL 746B
UL RTI, Mechanical with Impact 50.0 °CUL 746B
UL RTI, Mechanical without Impact 50.0 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.00 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 5VB
@Thickness >=2.50 mm
UL 94
 5VA
@Thickness >=2.50 mm
UL 94
Glow Wire Ignition Temperature 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 850 °C
@Thickness 1.00 mm
IEC 60695-2-13
 850 °C
@Thickness 2.00 mm
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 260 - 305 °C
Zone 3 270 - 310 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 75.0 - 105 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82407 / 290354

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.