LNP STAT-KON DE0029EF compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Flame Retardant, Electrically Conductive, Easy Molding. Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Electrically Conductive,Easy Molding Information provided by SABIC |