MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
High-Strength Yellow Brass, UNS C86500, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Shrinkage in Solidification, Drossing; Medium – Fluidity; Low – Casting Yield, Effect of Section Size, Gassing

Fabrication Properties: Fair Suitability – Soldering, Brazing; Poor Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Weld Guns; Brackets; Electrical Hardware; Electrical Hardware; Forming Dies for Wood Pulp Industry; Frames; Gears; Hooks; Lever Arms; Machinery; Machinery Parts (Substituted for Steel and Malleable Iron); Machinery Parts requiring High Strength; Pressing Dies for Wood Pulp; Struts; Wear Rings for Pressing Dies for Wood Pulp Industry; Boat Parts; Clamps; Covers for Marine Hardware; Propellers for salt and fresh water; Rudders

Applicable Specifications: As Centrifugal Cast - Castings ASTM B271/B271M, Castings AMS 4860, Castings SAE J462, Castings SAE J461; As Continuous Cast – Castings ASTM B505/B505M; As Die Cast – Castings ASTM B176; As Sand Cast – Castings AMS 4860, SAE J462, Castings ASTM B584, Castings SAE J461, Castings ASTM B763/B763M; Ingot - ASTM B30, FEDERAL QQ-C-523

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.301 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 65.0 ksifor Standard
Tensile Strength, Yield >= 25.0 ksifor Standard, 0.5% Ext
Elongation at Break >= 20 %for Standard
Tensile Modulus 15000 ksi
Machinability 26 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000780 ohm-cm22% IACS
Magnetic Permeability 1.09Field Strength 16 kA/m
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µin/in-°F
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 49.6 BTU-in/hr-ft²-°F
Melting Point 1583 - 1616 °F
Solidus 1583 °F
Liquidus 1616 °F
Shrinkage 2.08 %Patternmaker's Shrinkage (4/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.50 - 1.5 %
Copper, Cu 55 - 60 %
Iron, Fe 0.40 - 2.0 %
Lead, Pb <= 0.40 %
Manganese, Mn 0.10 - 1.5 %
Nickel, Ni <= 1.0 %
Tin, Sn <= 1.0 %
Zinc, Zn 36 - 42 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC86500x1 / 293170

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.