MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ COLORCOMP™ Compound G1000 Polysulfone (PSU)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: LNP COLORCOMP G1000 compound is based on unfilled Polysulfone (PSU) resin. Added features of this grade include: Transparent.

Features: Aesthetics and Appearance,Custom Color,Transparent

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Density 1.24 g/ccISO 1183
Water Absorption 0.40 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0500 %Injection Molding
 0.300 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527
 70.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 76.0 MPa50 mm/min; ISO 527
Elongation at Break 50 - 100 %5 mm/min; ASTM D638
Elongation at Yield 5.9 %50 mm/min; ISO 527
Tensile Modulus 2480 MPa50 mm/min; ASTM D638
 2500 MPa1 mm/min; ISO 527
Flexural Strength 106 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 115 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2500 MPa2 mm/min; ISO 178
 2690 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 69.0 JASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+17 ohm-cmASTM D257
Dissipation Factor 0.00070
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0060
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=4.50 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
 15 - 30 arcs
@Thickness >=6.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 61.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 62.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 183 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 170 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 174 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 160 °CUL 746B
UL RTI, Mechanical with Impact 140 °CUL 746B
UL RTI, Mechanical without Impact 160 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 V-0
@Thickness >=4.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 340 - 350 °C
Zone 3 350 - 360 °C
Melt Temperature 360 - 370 °CInjection Molding
Mold Temperature 150 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80556 / 288503

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.