Advantages:- Can control the rheological property of solvent based resin system
- Enhance the viscosity and consistency
- Provide pseudoplastic flowability
- Can renew viscosity after work and can control sagging problem
- Prevent subsiding of pigment and filler
- Liquid additive, easy to be operated
- Don’t have adverse effect to layer adhesion
- No negative effect to pseudo viscosity
Applications: - Acrylic resin system
- Solvent based PU resin series
- Oil based epoxy resin series
- Amino resin series
- Wood paint series
- Paint for constructional field
- Industrial paint
- Paint for boat and anti-corrosion
Information provided by Go Yen Chemical |