MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F584™/181 Style Modified Epoxy Resin/Fiberglass Fabric
Categories: Polymer; Thermoset; Epoxy

Material Notes: Wet is 30 days of humidity conditioning at 160°F (71°C) and 95% relative humidity.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 207 MPa30000 psiDry, Open hole tensile strength
 221 MPa32000 psiCompression after impact strength, The energy of impact was 960 in-lb/in, Dry, [(0°/90°), (±45°)]6s
 269 MPa
@Temperature 93.3 °C
39000 psi
@Temperature 200 °F
Dry
 379 MPa
@Temperature 23.9 °C
55000 psi
@Temperature 75.0 °F
Dry
Elongation at Break  1.32 %
@Temperature 93.3 °C
1.32 %
@Temperature 200 °F
Dry
 1.68 %
@Temperature 23.9 °C
1.68 %
@Temperature 75.0 °F
Dry
Tensile Modulus  20.7 GPa
@Temperature 93.3 °C
3000 ksi
@Temperature 200 °F
Dry
 22.8 GPa
@Temperature 23.9 °C
3300 ksi
@Temperature 75.0 °F
Dry
Compressive Strength  365 MPa
@Temperature 93.3 °C
53000 psi
@Temperature 200 °F
Wet
 552 MPa
@Temperature 23.9 °C
80000 psi
@Temperature 75.0 °F
Dry
Compressive Modulus  24.1 GPa
@Temperature 93.3 °C
3500 ksi
@Temperature 200 °F
Wet
 25.5 GPa
@Temperature 23.9 °C
3700 ksi
@Temperature 75.0 °F
Dry
Bearing Yield Strength 0.648 MPa94.0 psiDry, [(0°/90°), (±45°)]2s
 
Processing PropertiesMetricEnglishComments
Shelf Life  3.00 Month
@Temperature 4.00 °C
3.00 Month
@Temperature 39.2 °F
 6.00 Month
@Temperature -18.0 °C
6.00 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9129 / 322285

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.