MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL® A 218 MT15 V25 is recommended in all industrial parts, offering a good combination between thermal and mechanical properties. This grade is commonly used in the automotive industry to mould large parts with a low warpage, such as: rocker cover, car body parts, engine covers. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183/A
Water Absorption 1.4 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0054 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0065 cm/cm
Linear Mold Shrinkage, Transverse 0.012 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527 Type 1A
Elongation at Break 2.4 %ISO 527 Type 1A
Tensile Modulus 9000 MPaISO 527 Type 1A
Flexural Modulus 8500 MPaISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²ISO 180/1A
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+15 ohm-cmIEC 60093
Surface Resistance 5.00e+14 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 425 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
1210
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY

PRHOD616 / 137847

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.