Description: K-1010e is an expandable polystyrene grade containing pentane as a blowing agent. The products are delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3. K-1010e is available in 1050 kg octabins. Applications: The properties of K-1010e make it suitable for the production of thin-walled shape-moulded products as well as heavy insulation board by block moulding. Information provided by BEWi Synbra |