MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical ZINC STANNATE(Z.S) Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 12036-37-2

Advantages:

  • Excellent flame retardant and smoke suppressant
  • Non-toxic, the non-irritating for breathing system and skin
  • The ideal replacement of Sb2O3, and zinc stannate is be used by domestic plastic plants years after years under the requirements of national environmental protection
  • Great heat stability, heat resistance to 600?
  • Widely application
  • Zinc hydroxystannate only can use for the materials which operated at temperature under 180?, and zinc stannate can apply to any polymers
Applications:
  • Plastic products and high-end plastic product
  • PU(Polyurethane),?PVC(PolyVinyl Chloride) products which are processing
  • Rigid or soft PVC?FRLS composite cables
  • EVA?HFFR composite wires and cables
  • Polyester resin
  • Epoxy resin
  • Nylon
  • Chlorinated rubber
  • Alkyd resin paint

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 g/cc0.141 lb/in³
Grain Size 10 µm10 µm>98%
Molecular Weight 232.07 g/mol232.07 g/mol
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %Free
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl <= 0.30 %<= 0.30 %
Tin, Sn >= 46 %>= 46 %
Zinc, Zn >= 26 %>= 26 %
 
Descriptive Properties
AppearanceWhite powder
Dissolving temperature>270°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN153 / 266461

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.