Characteristic:- Optimal balance of physical properties
- High impact strength
- Good flow
- Excellent processability
Applications: Computer/ TV/ telephone housing, toys, kitchen appliances, electronic products outer covering, extruded film, OA appliances and items, battery shell, daily suppliesInformation provided by Go Yen Chemical |