MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP

Material Notes: PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.

This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D 792
Density 1.17 g/ccISO 1183
Moisture Absorption at Equilibrium 0.010 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.010 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 265 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 11 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527
 63.0 MPaType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 61.0 MPaType I, 50 mm/min; ASTM D 638
 61.0 MPa50 mm/min; ISO 527
Elongation at Break 110 %Type I, 50 mm/min; ASTM D 638
 125 %50 mm/min; ISO 527
Elongation at Yield 6.0 %Type I, 50 mm/min; ASTM D 638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2130 MPa50 mm/min; ASTM D 638
 2300 MPa1 mm/min; ISO 527
Flexural Strength 89.0 MPa2 mm/min; ISO 178
Flexural Yield Strength 86.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2150 MPa1.3 mm/min, 50 mm span; ASTM D 790
 2210 MPa2 mm/min; ISO 178
Izod Impact, Notched 81.0 J/m
@Temperature -30.0 °C
ASTM D 256
 88.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 67.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 69.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 71.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 72.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 113 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 105 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 122 °CRate B/50; ISO 306
 123 °CRate B/50; ASTM D 1525
 124 °CRate B/120; ISO 306

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABIC6303 / 120191

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.