System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Medium Density (MDPE)
;
Medium Density Polyethylene (MDPE), Molded
Material Notes:
Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.
Applications:
Roll-out cart lids.
Data provided by the manufacturer.
Key Words:
Medium Density Polyethylene
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.941
g/cc
ASTM D792
ESCR 100% Igepal®
30
hour
F50, Condition A, ASTM D1693
Melt Flow
11
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
63
ASTM D2240
Tensile Strength, Yield
19.0
MPa
ASTM D638
Elongation at Break
400 %
ASTM D638
Flexural Modulus
0.600
GPa
ASTM D790
Thermal Properties
Original Value
Comments
Vicat Softening Point
119
°C
ASTM D1525
Processing Properties
Original Value
Comments
Melt Temperature
170
-
215
°C
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 2272 Polyethylene, Injection Grade
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin
PEHN1K / 35569
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.