This cast polyamide incorporates a liquid lubricant and is self-lubricating in the truest sense of the word. This material, which was developed especially for heavy-duty, slow-moving non-lubricated sliding elements, significantly enhances the range of possible applications of polyamides thanks to its low coefficient of friction (up to 50 % less) and high wear resistance (up to 10 times higher).Information provided by Angst + Pfister |