MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

RAMPF RAKU® TOOL IE-3665 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Impact resistant polyurethane

Key Properties:

  • Excellent physical properties
  • Free of mercury, MOCA or MDI
Applications:
  • For hand-batch or vacuum assisted casting methods
Cure 1: 24 hours at 77°F + 16 hours at 180°F
Cure 2: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³Hardener; ASTM D-792
 1.08 g/cc0.0390 lb/in³Cure 1; ASTM D-792
 1.08 g/cc0.0390 lb/in³Cure 2; ASTM D-792
 1.09 g/cc0.0394 lb/in³Resin; ASTM D-792
Viscosity 100 cP100 cPHardener; ASTM D-2393
 2000 cP2000 cPMix; ASTM D-2393
 3000 cP3000 cPResin; ASTM D-2393
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45 - 5545 - 55Cure 1; ASTM D-2240
 45 - 5545 - 55Cure 2; ASTM D-2240
Tensile Strength 15.9 MPa2300 psiCure 2; ASTM D-638
 16.5 MPa2400 psiCure 1; ASTM D-638
Elongation at Break 210 %210 %Cure 1; ASTM D-638
 275 %275 %Cure 2; ASTM D-638
Flexural Strength 241 MPa35000 psiCure 1; ASTM D-790
 310 MPa45000 psiCure 2; ASTM D-790
Flexural Modulus 2.139 GPa310.2 ksiCure 2; ASTM D-790
 2.368 GPa343.5 ksiCure 1; ASTM D-790
Izod Impact, Notched 5.34 J/cm10.0 ft-lb/inCure 1; ASTM D-256
 5.34 J/cm10.0 ft-lb/inCure 2; ASTM D-256
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 240 min2.00 - 4.00 hourMix, Demold time
Gel Time 10.0 - 14.0 min10.0 - 14.0 minMix
 
Descriptive Properties
AspectTranslucent AmberCure 1
 Translucent AmberCure 2
Mix Ratio100:20Resin: Hardener, Weight
 100:20Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF016 / 317616

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.