MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL GTX™ Resin GTX951W Polyphenylene Ether + PA (PPE+Nylon) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 951W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, excellent chemical resistance, high melt flow, and added mold release. NORYL GTX951W resin was designed for automotive under-the-hood applications such as power distribution boxes, relay boxes, and junction boxes.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Good Processability,Good Moldability,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Moisture Absorption 0.0700 %0.0700 %Injection Molding
Melt Flow  24 g/10 min
@Load 2.16 kg,
Temperature 280 °C
24 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ASTM D1238
 65 g/10 min
@Load 5.00 kg,
Temperature 280 °C
65 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ASTM D638
Elongation at Break 55 %55 %50 mm/min; ASTM D638
Flexural Strength 100 MPa14500 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.45 GPa355 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 211 J156 ft-lbASTM D256
 100 J
@Temperature -30.0 °C
73.8 ft-lb
@Temperature -22.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 22.4 kV/mm
@Thickness 1.60 mm
569 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
@Thickness 6.40 mm
383 °F
@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.20 mm
HB
@Thickness 0.0472 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 300 °C518 - 572 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82181 / 290128

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.