MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Caplinq Spectracarb™ 2050A-1550 GDL Porous Carbon-Carbon Paper
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: SpectracarbTM 2050A-1550 GDL is a heavy duty porous graphitized carbon /carbon sheet with low compressibility and with general utility for a range of PEM fuel cell applications, including both commercial and military applications. Special 1550-HT grade also available for use in PAFS fuel cells for higher electrical and thermal conductivities, as well as increased corrosion resistance.

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.500 g/cc0.0181 lb/in³Geometric
Porosity 78 %78 %
Permeability 3535[cfm/ft2], through-plane, Air
Thickness 351 microns13.8 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 40.0 MPa5800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00540 ohm-cm0.00540 ohm-cmin-plane
 0.0150 ohm-cm
@Pressure 0.200 MPa
0.0150 ohm-cm
@Pressure 29.0 psi
[O·cm2], through-plane
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  3.40 W/m-K
@Temperature 25.0 °C
23.6 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
through-plane
 3.60 W/m-K
@Temperature 100 °C
25.0 BTU-in/hr-ft²-°F
@Temperature 212 °F
through-plane
 20.7 W/m-K
@Temperature 25.0 °C
144 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
in-plane
 24.2 W/m-K
@Temperature 100 °C
168 BTU-in/hr-ft²-°F
@Temperature 212 °F
in-plane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCAPL1021 / 256021

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.