GOYENCHEM-OP1200, design by GO YEN CHEMICAL INDUSTRIAL CO. LTD., is an innovation creation for high performance polyamides for E&E applications. Intro: GOYENCHEM-OP1200, design by GO YEN CHEMICAL INDUSTRIAL CO. LTD., is an innovation creation for high performance polyamides for E&E applications. GOYENCHEM-OP1200 is a white, fine-grained powder based on an organic phosphinate. The product is nonhygroscopic and it is insoluble in water and organic solvents that can enhance the manufacture process and the quality of finished products. It can be applied in polyamide, polyester or various kinds of raw materials for engineering plastics. High processing temperatures and the strong trend of manufacturing processing put a lot of requirements on a suitable flame retardant. GOYENCHEM-OP1200 is the best choice of non-halogen flame retardant that can cope with the demanding process and stringent requirements of this high end segment of engineering plastics. Advantages: - With perfect heat-resistance and anti-heat decomposition.
- Insoluble in water and general organic solvent.
- With outstanding water resistance
- With anti-ion migration ability and comprehensive mechanical properties
- With excellent electrical and mechanical properties.
- With high effective phosphorus element.
- With outstanding dispersion in resin and organic solvent.
Applications:- 3L-FCCL without migration ability
- Epoxy resin electrical pouring sealant
- Label adhesive
- Epoxy resin printed circuit board and other advanced application Non-halogen flame retardant
- Flame retardant for various electronic products
- Thermosetting and thermoplastic products
- Hot melt adhesive, coating, sealant
- Nylon?SEBS?PET?TPU engineering plastic and elastomers
Information provided by Go Yen Chemical |