Product Description: High flow, Electroplating Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: High Flow; Platable Uses: General Purpose RoSH Compliance: RoSH Compliant Part Marking Code (ISO 11469): >ABS+PC< Resin ID (ISO 1043): >ABS+PC< Information provided by Chi Mei Corporation |