MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Pyrotek Ceramite® SFW Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Ceramite® SFW is a cast refractory containing white cement, and based on fused silica material. This refractory is naturally non-wetting and formulated especially for use with high silicon alloys, typically foundry alloys. Products cast from this refractory are mainly used in the industry for casting launders, ceramic filter boxes and casting table modules. The aggregates in this formulation have a maximum grain size of approximately 5 millimeters (0.20 inches) and the material supports a maximum service temperature of up to 1000°C (1832°F).

Benefits:

  • Low thermal expansion
  • Low thermal conductivity
Applications:
  • Casting launders
  • Ceramic filter bowls
  • Casting table modules

Information provided by Pyrotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/cc
@Temperature 600 °C
 1.80 g/cc
@Temperature 20.0 °C
Grain Size <= 5000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00400 GPa
@Temperature 20.0 °C
Cold
 0.00500 GPa
@Temperature 600 °C
Cold
 0.00600 GPa
@Temperature 850 °C
Cold
 0.00600 GPa
@Temperature 1000 °C
Cold
Compressive Strength 24.0 MPa
@Temperature 20.0 °C
Cold
 37.0 MPa
@Temperature 600 °C
Cold
 42.0 MPa
@Temperature 1000 °C
Cold
 44.0 MPa
@Temperature 850 °C
Cold
Abrasion 19.9
@Temperature 600 °C
[cm^3]
 21.8
@Temperature 20.0 °C
[cm^3]
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.600 W/m-K
@Temperature 300 °C
 0.600 W/m-K
@Temperature 600 °C
 0.700 W/m-K
@Temperature 900 °C
Maximum Service Temperature, Air 1000 °C
Shrinkage -0.200 %
@Temperature 20.0 - 850 °C
 
Descriptive Properties
Permanent Linear Change0.7%20-850°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CPYRO520 / 199542

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.