MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veradel® 3600RP Polyethersulfone (PESU), Lower molecular weight
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Lower molecular weight with a higher level of functionality

Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing into solutions and to improve adhesion to substrates when used as a coating.

Veradel® 3600RP r-PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water and mineral acids. Cast films or coatings of r-PESU are transparent and have additional desirable properties, including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance.

Veradel® r-PESU polymers are available in two molecular weight regimes. Veradel® 3000RP is a high molecular weight sulfone polymer with a relatively low level of functionality while Veradel® 3600RP has a lower molecular weight sulfone polymer (approximately half the molecular weight of the Veradel® 3000RP) with roughly 3-5 times higher level of functionality. The differences in molecular weight results in highly varied levels of viscosity, when measured under similar conditions.

Typical applications include high-temperature coating formulations and specialty adhesives.

All Veradel® r-PESU polymers are produced at Solvay's state-of-the-art, world-scale facility in Panoli, India under ISO 9001:2000 and ISO 14001:2004 certified quality management systems.

Markets/Uses: Coatings / High Performance Coatings / Abrasion Resistant Coatings; Coatings / High Performance Coatings / Corrosion Resistant Coatings; Coatings / High Performance Coatings / High-Temperature Coatings; Coatings / High Performance Coatings / Primers for Non-Stick Coatings

Applications: Adhesives; Binder; Coating Applications

Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Flow; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Low Molecular Weight; Medium Rigidity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 250 µm
Viscosity 80 - 560 cPSolution Viscosity; ASTM D445
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 90.0 MPaASTM D638
Elongation at Yield 6.5 %ASTM D638
Tensile Modulus 2700 MPaASTM D638
Flexural Strength 2.60 MPaASTM D790
Flexural Modulus 2600 MPaASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 220 °CASTM E1356
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorTransparent - Slight Yellow
FormsGranules; Powder
ProcessingCoating; Solution Processing; Spraying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4600 / 280400

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.