PEXIDAN® H/T is a low density flame-retardant XLPE system curable by moisture and consists of a silane pregrafted base compound A-3001 and a flame-retardant catalyst masterbatch CAT-012FR. Mixed and extruded in the proper proportions (67/33) this mixture results in a material curable by exposure to 70-95°C hot water or even ambient moisture. PEXIDAN® H/T is listed with CSA for AWM and CL1251, CL1252 & CL1503, and for UL AWM styles 3173 and 3321. PEXIDAN® H/T is halogenated but is RoHS-compliant.Information provided by SACO AEI Polymers. |