MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lion TrileneĀ® 65D Liquid EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Trilene 65D is an Ethylene-Propylene-Dicyclopentadiene (EPDM) elastomer dispersed and stabilized in water. It is randomly polymerized to produce a polyolefinic polymer with a stable, saturated hydrocarbon backbone and side group unsaturation to enable crosslinking. It has excellent thermal and oxidation stability under normal conditions. Trilene 65D can be used in a variety of water-based applications such as coatings, adhesives, inks, caulks, and sealants.

Unique Features:

  • Excellent UV, heat, oxidation and chemical stability
  • Good mechanical strength
  • Manageable viscosity at room temperature
  • Low odor and water clean-up
  • Crosslinked with metal driers, peroxides, or UV light
  • Compatible with a variety of other latex resins
  • No Volatile Organic Content (VOC)
Applications:
  • Industrial Coatings: Primary binder or modifier for applications such as roofing, industrial maintenance and institutional paints
  • Adhesives & sealants: Primary binder or modifier for applications such as pressure sensitive adhesives and industrial caulks
  • Inks & overnight varnishes: Modifier for applications in laminating inks and overprint varnishes

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D4052
Solids Content 50 - 55 %in water
pH 8.0 - 9.0ASTM D7946
Brookfield Viscosity 5600 cPASTM D2196
Molecular Weight 11300 g/molMn
 47000 g/molMw
 
Descriptive Properties
ColorMilky white
Content0.1Degree of unsaturation, Dicyclopentadiene
 0.45Propylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLION058 / 317967

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.