MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP30LTE-LO Black Two component epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Good flow properties
  • Very low shrinkage
  • Withstands 1,000 hours 85°C/85% RH
  • Passes NASA low outgassing
Product Description: Master Bond EP30LTE-LO Black is a two part epoxy, adhesive, sealant, coating and encapsulating system featuring a low coefficient of thermal expansion (CTE). It has an easy to use 10:1 mix ratio by weight and upon mixing, flows smoothly and readily. It has several curing schedules with an optimum being overnight at room temperature followed by 4-8 hours at 150-200°F. This epoxy system has superior dimensional stability and low shrinkage upon curing of less than 0.01%. Its CTE is 15-18 x 10-6 in/in/°C. EP30LTE-LO Black bonds well to a wide variety of substrates including metals, glass, ceramics and many rubbers and plastics. This high modulus epoxy is thermally conductive and electrically insulating. It has good chemical resistance to water, oils and fuels. It is cryogenically serviceable with a temperature range extending from 4K to +250°F. Part A is black and Part B is clear. Master Bond EP30LTE-LO Black is used in aerospace, optical, electronic, specialty OEM and other applications where an ultra low CTE, low outgassing, and a black colored system is required. Some applications include mounting optics and sealing fibers into ferrules, as an underfill in flip chip devices, as well as a heat sinking adhesive in situations where thermal management is required.

Product Advantages:

  • Easy to mix and dispense
  • Low shrinkage upon curing
  • Thermally conductive, electrically insulating
  • Passes NASA low outgassing
  • Low coefficient of thermal expansion

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 290 - 500 cP290 - 500 cPPart B
 35000 - 70000 cP35000 - 70000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090after 1,000 hours 85°C/85% RH
 85 - 9585 - 95
Tensile Strength 41.4 - 48.3 MPa6000 - 7000 psi
Tensile Modulus 3.79 - 4.14 GPa550 - 600 ksi
Compressive Strength 165 - 179 MPa24000 - 26000 psi
Adhesive Bond Strength 6.89 - 8.27 MPa1000 - 1200 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.5
@Frequency 60 Hz
4.5
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 18.0 µm/m-°C8.33 - 10.0 µin/in-°F
Thermal Conductivity 1.01 - 1.30 W/m-K7.00 - 9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -269 °C-452 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
Option 3
 240 - 480 min
@Temperature 65.6 - 93.3 °C
4.00 - 8.00 hour
@Temperature 150 - 200 °F
Optimal: Overnight at 75°F followed by 4-8 hours at 150°F to 200°F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Option 2
Working Life 45.0 - 75.0 min45.0 - 75.0 min
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Monthin original unopened containers
 
Descriptive Properties
Mixing ratio10:1 by weightPart A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5919 / 306808

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.