MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HB Chemical Cilbond® 12E Primer
Categories: Other Engineering Material

Material Notes: Cilbond 12E primer gives excellent adhesion to metals, including mild steel, cast iron, phosphated steel, chromated steel, stainless steel, aluminum, brass, nickel, zinc, etc. and polar engineering thermoplastics, such as PPO, PPS, PES, PEEK, PET, PBT, nylons and theromset plastics, such as UF, PF, RF, MF and GRP/FRP and epoxy resins. Cilbond 12E is used under bonding agents such as Cilbond 80ET to bond a vast range of elastomers to metals and plastics during the molding process – See also the Cilbond 80ET Technical Data Sheet. Cilbond 12E may also be used as a One-Component vulcanizing and post-vulcanising bonding agent for NR, SBR, CR, CSM and Vamac® G compounds. In-Service Benefits: As a Primer, Cilbond 12E has excellent resistance to extreme environments including fluids (for example, glycols and brake fluids) and high temperatures of up to 390°F and low temperatures down to -58°F. The use of Cilbond 12E as a Primer under Cilbond 24 gives bonds with the ultimate in environmental resistance and maintains the exceptional heat and fluid resistance (particularly glycol) associated with Cilbond 24. When Cilbond 12E is used as a Primer under Cilbond 80ET, bonded components benefit from superior salt-spray and hot-fluid resistance. Cilbond 12E may show improved heat resistance when used as a primer under Cilbond 65W for some grades of VMQ and FKM. Cilbond 12E should be considered as a Primer under Cilbond 10E for superior heat resistance when bonding NBR and HNBR.

Information provided by HB Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/cc
Solids Content 17.1 %17.1 %
Volatiles 76 %76 %
Viscosity Measurement 3030[sec], DIN 4 Cup
 17
@Temperature 25.6 °C
17
@Temperature 78.0 °F
[sec], No 3 Zahn Cup
 
Thermal PropertiesMetricEnglishComments
Flash Point 2.22 °C36.0 °FAbel Pensky
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceGrey Liquid
Bonding Temperature265-455°F
Content0.612HAP
In-Service Temperature Resistance-58-390°F
Typical Coverage815 ft2/US galat 15 microns/0.6 mil (dry)
VOC0.76

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBCHEM023 / 317442

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.