MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL 731 PPE+HIPS (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: NORYL 731 is an unfilled material, with a Vicat B/120 of 140C according ISO 306. NORYL 731 is a general purpose material with good balance of Strength, Impact and Flow. NORYL 731 is available in all colours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmon Tensile Bar; SABIC Method
Melt Index of Compound 8.0 g/10 min
@Load 5.00 kg,
Temperature 280 °C
MVR [cm^3/10 min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, H358/30 100 MPaISO 2039-1
Tensile Strength at Break 50.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
Elongation at Break 30 %50 mm/min; ISO 527
Elongation at Yield 5.0 %50 mm/min; ISO 527
Tensile Modulus 2300 MPa1 mm/min; ISO 527
Flexural Yield Strength 75.0 MPa2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 65CS-17, 1 kg; SABIC Method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.6
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
IEC 60250
 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.220 W/m-KISO 8302
Hot Ball Pressure Test <= 133 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 115 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 135 °CRate B/50; ISO 306
 140 °CRate B/120; ISO 306
 145 °CRate A/50; ISO 306
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 HB
@Thickness 3.00 mm
UL 94
Oxygen Index 22 %ISO 4589
Glow Wire Flammability Index 750 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Descriptive Properties
Ball Pressure Test, 125°C +/- 2°CPASSESIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® L-1250Z Polycarbonate, Weather Resistant
Syensqo (Solvay Specialty Polymers) Algoflon® A.30 PTFE (Polytetrafluoroethylene)
Mitsubishi Xantar® RX 2125 Polycarbonate
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade

PSABI55448 / 155494

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.