MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC FLEX NORYL™ Resin WCV072 Polyphenylene Ether + TPE (PPE+TPE) (Americas)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCV072 resin is a flexible, non-reinforced extrusion grade of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE) with a Shore D Hardness rating of 72. FLEX NORYL WCV072 resin was developed for evaluation in automotive wire + cable applications requiring ISO6722 Class A or B. It exhibits ultra-thin wall capability, good scratch abrasion and pinch resistance, high dimensional stability, low shrinkage and warpage, very low water absorption, chemical resistance, and good dielectric strength. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Density 1.03 g/ccISO 1183
Moisture Absorption 0.0200 %Wire Coating Extrusion
 0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.12 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Melt Flow 13.8 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 41.0 MPa50 mm/min; ASTM D638
 42.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 43.0 MPa50 mm/min; ASTM D638
 44.0 MPa50 mm/min; ISO 527
Elongation at Break 46 %50 mm/min; ISO 527
 83 %50 mm/min; ASTM D638
Elongation at Yield 11 %50 mm/min; ISO 527
 15 %50 mm/min; ASTM D638
Tensile Modulus 1710 MPa50 mm/min; ASTM D638
 1750 MPa1 mm/min; ISO 527
Flexural Strength 53.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 59.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 1550 MPa1.3 mm/min, 50 mm span; ASTM D790
 1740 MPa2 mm/min; ISO 178
Izod Impact Notched 309 JASTM D256
 67.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 36.0 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 33.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 45.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 111 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 92.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 114 °CRate B/50; ASTM D1525
 114 °CRate B/50; ISO 306
 117 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 15.0 - 80.0 °CWater Bath Temperature
 250 - 285 °CNeck Temperature
Feed Temperature 210 - 260 °C
Middle Barrel Temperature 230 - 285 °C
Die Temperature 250 - 285 °CWire Coating Extrusion
Melt Temperature 250 - 285 °CWire Coating Extrusion
Head Temperature 250 - 285 °CCross-head Temperature
 250 - 285 °C
Wire Preheat Temperature 80.0 - 150 °C
Drying Temperature 60.0 - 80.0 °CWire Coating Extrusion
Dry Time 4.00 - 6.00 hourWire Coating Extrusion
 12.0 hourCumulative; Wire Coating Extrusion
Screw Speed 15 - 40 rpm
 
Descriptive Properties
Cooling Water Air Gap100-200 mm
Extruder Length/Diameter Ratio (L/D)22:1 to 26:1
Screen Pack150-100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82108 / 290055

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.