MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-PLA-SERIES Environmental-Friendly Biodegradable Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Characteristic:
  • Excellent dispersion. No falling off powder even at high ratio dosage.
  • To decrease heat generation.
  • No smoke and oil dripping when burning. No destroy to the incinerator.
  • To provide prominent printability for products.
  • To increase the surface smoothness and luster of products.
  • To reduce the usage of white pigment because of great opacity.
  • Environmental-friendly and also cut down the cost of environment.
Applications:
  • Garbage bags
  • Inner film for laminated paper bags
  • Shopping bags
  • Blow molding products
  • Adhesive tape

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/cc
Melt Flow 1.7 g/10 min
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %
 
Descriptive Properties
Appearancegranule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN793 / 267101

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.