MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® HF S/C-UV Moisture Cure XLPE Low Smoke Zero Halogen Jacket
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® HF S/C-UV is a high performance, low smoke halogen-free, flame retardant, colorable 105°C rated XLPE jacketing system curable by moisture. It consists of a silane pre-grafted base compound SX-0652 and a catalyst masterbatch CM540U/1. Mixed and extruded in the proper proportions (95:5), the two components result in a material that is crosslinkable by exposure to 90°C hot water. Used in conjunction with PEXIDAN® HF X/T UL 44 LSZH insulated conductors, the completed cable would meet LSZH requirements and is FT4 and UL1685-capable. Cables jacketed with PEXIDAN® HF S/C-UV are intended to be marked SUNRES. PEXIDAN® HF S/C-UV is both REACH and RoHS-compliant.

Applications:

  • UL1277 Jacket for Single- and Multi-Conductor Tray-Rated LV and MV Cables
  • Low Smoke Zero Halogen Hazardous Industrial Environments
  • Petrochemical | Transit | Offshore Oil Platforms | Substation Control

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 7.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
ASTM D1238
Deformation <= 10 %
@Load 2.00 kg,
Temperature 121 °C
UL 1277 / UL 2556
Storage Temperature <= 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 97
@Time 1.00 sec
ASTM D2240
Hardness, Shore D 58
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1810 psiUL 1277 / UL 2556
 >= 1176.5 psi
@Temperature 75.0 °C
After 60 days oil (OILRES II); UL 1277 / UL 2556
 >= 1303.2 psi
@Temperature 100 °C,
Time 346000 sec
Oil (OILRES I); UL 1277 / UL 2556
 >= 1538.5 psi
@Temperature 136 °C,
Time 605000 sec
after thermal ageing; UL 1277 / UL 2556
 >= 1538.5 psi
@Temperature 121 °C,
Time 605000 sec
thermal ageing; UL 1277 / UL 2556
Elongation at Break 253 %UL 1277 / UL 2556
 >= 164.45 %
@Temperature 75.0 °C
After 60 days oil (OILRES II); UL 1277 / UL 2556
 <= 40 %
@Temperature 150 °C,
Time 900 sec
Hot, 0.2 N/mm2 load; UL 1277 / UL 2556
 >= 177.1 %
@Temperature 136 °C,
Time 605000 sec
after thermal ageing; UL 1277 / UL 2556
 >= 177.1 %
@Temperature 121 °C,
Time 605000 sec
thermal ageing; UL 1277 / UL 2556
 >= 247.94 %
@Temperature 100 °C,
Time 346000 sec
Oil (OILRES I); UL 1277 / UL 2556
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -30.0 °C3 min in Methanol; ASTM D638
Smoke Density <= 50Flaming, corrected; ASTM E662
 <= 70Non-flaming, corrected; ASTM E662
 <= 1.0
@Time 240 sec
Flaming; ASTM E662
 <= 2.0
@Time 240 sec
Non-flaming; ASTM E662
Oxygen Index 35 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 154 - 171 °Cbarrel zones
Die Temperature 179 °C
Head Temperature 177 °C
 
Descriptive Properties
Degree of Crosslinking77%ASTM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO006 / 249373

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.