MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon Cadox L-30a VR Methyl ethyl ketone peroxide
Categories: Other Engineering Material

Material Notes: Special purpose catalyst (including vanishing red cure indicator) used for curing tooling gel coats and promoted unsaturated polyester resins in warmer climates. Low-hydrogen peroxide content reduces gelcoat porosity and provides improved curing of vinylester resins.

CAS number: 1338-23-4

EINECS/ELINCS No.: 215-661-2

Applications: Cadox L-30a VR can be used in place of Cadox L-50a or Cadox L-50a VR wherever a more dilute solution of methyl ethyl ketone peroxide (MEKP) is desired. Cadox L-30a VR is a special purpose ‘summer catalyst’ for use in warmer shop environments. Cadox L-30a VR offers all the advantages of a red MEKP, except red parts. The VR series of products includes a red indicator system that virtually disappears during cure. The red is there when you need it, but not in the finished product. Visualize Hot & Cold Spots, Shrinkage Problems, Mass Effects, Thermal Effects of Core Materials and Dead Flow Zones in applications like Vacuum Infusion.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Brookfield Viscosity 15 cP15 cPLVT, UL adapter, spindle 1.6 rpm
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Descriptive Properties
AppearanceRed liquid
Content(%)5.3Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY458 / 285981

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.