MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow

Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin with improved flow. It is also a PPA

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmDAM; ISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 135 MPa50%RH; ISO 527-1/-2
 145 MPaDAM; ISO 527-1/-2
Elongation at Break 1.9 %50%RH; ISO 527-1/-2
 2.1 %DAM; ISO 527-1/-2
Tensile Modulus 10700 MPaDAM; ISO 527-1/-2
 11300 MPa50%RH; ISO 527-1/-2
Flexural Strength 200 MPa50%RH; ISO 178
 225 MPaDAM; ISO 178
Flexural Modulus 9800 MPaDAM; ISO 178
 10800 MPa50%RH; ISO 178
Charpy Impact Unnotched 40.0 kJ/m²50%RH; ISO 179/1eU
 45.0 kJ/m²DAM; ISO 179/1eU
 35.0 kJ/m²
@Temperature -30.0 °C
50%RH; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²DAM; ISO 179/1eA
 7.00 kJ/m²50%RH; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
50%RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°CDAM; ISO 11359-1/-2
 12.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
 18.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 62.0 µm/m-°CDAM; ISO 11359-1/-2
 60.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 95.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point 310 °CDAM; first heat; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 281 °CDAM; ISO 75-1/-2
UL RTI, Electrical 140 °C
@Thickness 0.400 mm
UL 746B
 140 °C
@Thickness 0.800 mm
DAM; UL 746B
 140 °C
@Thickness 1.50 mm
DAM; UL 746B
 140 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 V-0
@Thickness 0.400 mm
DAM; IEC 60695-11-10
Oxygen Index 37 %DAM; ISO 4589-1/-2
Glow Wire Test 700 °C
@Thickness 0.400 mm
DAM; IEC 60695-2-1/2
 775 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-1/3
 960 °C
@Thickness 0.400 mm
DAM; IEC 60695-2-1/2
 960 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-1/2
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PA6T/66-GF30FR<ISO 11469
 >PPA-GF30FR<SAE J1344
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
UL recognitionULDAM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Celanese Zytel® HTN 51G50HSL BK083 Polyphthalamide (PPA)

PZDSY5459 / 161286

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.