MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Red Brass, UNS C23000 (230 Brass), H00 Temper, Wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: 1/8 Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Spot Weld

Common Fabrication Processes: Blanking; Coining; Drawing; Etching; Forming and Bending; Heading and Upsetting; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical uses: Etching Parts; Trim; Weather Strip; Kick Plates; Badges; Coinage; Compacts; Costume Jewelry; Dials; Fire Extinguisher Cases; Lipstick Containers; Medallions; Nameplates; Plaques; Rouge Boxes; Tokens; Zippers; Conduit; Rotor Bars, AC Motors; Screw Shells; Sockets; Eyelets; Fasteners; Condenser Tubes; Fire Extinguishers; Flexible Metal Hose; Heat Exchanger Shells; Heat Exchangers; Pickling Crates; Pump Cylinder Liners; Radiator Cores; Tags; Tubing for Heat Exchangers; Tubing for Instrumentation; Fire Hose Couplings; Fittings; J-Bends; Pipe; Pipe Nipples; Pipe Service Lines; Pump Lines; Service Lines; Traps

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.316 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 ksi
@Thickness 2.03 mm
Elongation at Break 25 %
@Thickness 2.03 mm
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Fatigue Strength 20000 psi
@Thickness 2.03 mm,
# of Cycles 1.00e+8
Machinability 30 %
Shear Strength 35.0 ksi
@Thickness 2.03 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000460 ohm-cm37% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 92.0 BTU-in/hr-ft²-°F
Melting Point 1810 - 1880 °F
Solidus 1810 °F
Liquidus 1880 °F
Annealing Point 800 - 1350 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1450 - 1650 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 84 - 86 %
Iron, Fe <= 0.050 %
Lead, Pb <= 0.050 %
Zinc, Zn 13.9 - 16 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC23000x2 / 292896

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.