MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Filament AM9085F
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM™ AM9085F filament is a high performance polyetherimide blend product manufactured from ULTEM™ 9085 resin. It is available in black and natural (unpigmented) colors. It provides high heat resistance and mechanical strength, is UL94 V-0 compliant at 1.5 and 3.0 mm (Blue Cards are available on UL IQ Database), and meets FAR 25.853 and OSU 55/55 with low toxicity, smoke, and flame evolution.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.275 g/cc0.04606 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psi5 mm/min; ASTM D638
 62.0 MPa8990 psi5 mm/min; ASTM D638
 80.0 MPa11600 psi5 mm/min; ASTM D638
Elongation at Break 2.3 %2.3 %5 mm/min; ASTM D638
 5.1 %5.1 %5 mm/min; ASTM D638
 5.8 %5.8 %5 mm/min; ASTM D638
Tensile Modulus 2.176 GPa315.6 ksiXY ORIENTATION; ASTM D638
 2.439 GPa353.7 ksiZX ORIENTATION; ASTM D638
 2.555 GPa370.6 ksiXZ ORIENTATION; ASTM D638
Flexural Modulus 2.07 GPa300 ksi1.3 mm/min; ASTM D790
 2.126 GPa308.4 ksi1.3 mm/min; ASTM D790
 2.55 GPa370 ksi1.3 mm/min; ASTM D790
Izod Impact Notched 33.0 J24.3 ft-lbZX ORIENTATION; ASTM D256
 100 J73.8 ft-lbXZ ORIENTATION; ASTM D256
 104 J76.7 ft-lbXY ORIENTATION; ASTM D256
Izod Impact, Unnotched 1.31 J/cm2.45 ft-lb/inZX ORIENTATION; ASTM D256
 7.63 J/cm14.3 ft-lb/inXY ORIENTATION; ASTM D256
 10.03 J/cm18.79 ft-lb/inXZ ORIENTATION; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.07e+15 ohm-cm1.07e+15 ohm-cmXY ORIENTATION; ASTM D257
 1.10e+15 ohm-cm1.10e+15 ohm-cmXZ ORIENTATION; ASTM D257
Dielectric Constant  2.52
@Frequency 1e+9 Hz
2.52
@Frequency 1e+9 Hz
XY ORIENTATION; ASTM D150
 2.53
@Frequency 5.00e+8 Hz
2.53
@Frequency 5.00e+8 Hz
XY ORIENTATION; ASTM D150
 2.54
@Frequency 1e+8 Hz
2.54
@Frequency 1e+8 Hz
XY ORIENTATION; ASTM D150
 2.71
@Frequency 1e+9 Hz
2.71
@Frequency 1e+9 Hz
XZ ORIENTATION; ASTM D150
 2.72
@Frequency 5.00e+8 Hz
2.72
@Frequency 5.00e+8 Hz
XZ ORIENTATION; ASTM D150
 2.73
@Frequency 1e+8 Hz
2.73
@Frequency 1e+8 Hz
XZ ORIENTATION; ASTM D150
Dissipation Factor  0.00233
@Frequency 1e+8 Hz
0.00233
@Frequency 1e+8 Hz
XY ORIENTATION; ASTM D150
 0.0030
@Frequency 1e+8 Hz
0.0030
@Frequency 1e+8 Hz
XZ ORIENTATION; ASTM D150
 0.0040
@Frequency 1e+9 Hz
0.0040
@Frequency 1e+9 Hz
XY ORIENTATION; ASTM D150
 0.0040
@Frequency 1e+9 Hz
0.0040
@Frequency 1e+9 Hz
XZ ORIENTATION; ASTM D150
 0.0050
@Frequency 5.00e+8 Hz
0.0050
@Frequency 5.00e+8 Hz
XY ORIENTATION; ASTM D150
 0.00567
@Frequency 5.00e+8 Hz
0.00567
@Frequency 5.00e+8 Hz
XZ ORIENTATION; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 57.1 µm/m-°C31.7 µin/in-°FXY ORIENTATION; ASTM E831
 60.6 µm/m-°C33.7 µin/in-°FXZ ORIENTATION; ASTM E831
 62.1 µm/m-°C34.5 µin/in-°FZX ORIENTATION; ASTM E831
CTE, linear, Transverse to Flow 58.3 µm/m-°C32.4 µin/in-°FXY ORIENTATION; ASTM E831
 61.1 µm/m-°C33.9 µin/in-°FXZ ORIENTATION; ASTM E831
 62.9 µm/m-°C34.9 µin/in-°FZX ORIENTATION; ASTM E831
Deflection Temperature at 1.8 MPa (264 psi)  165 °C
@Thickness 3.20 mm
329 °F
@Thickness 0.126 in
unannealed; ASTM D648
 175 °C
@Thickness 3.20 mm
347 °F
@Thickness 0.126 in
unannealed; ASTM D648
 175 °C
@Thickness 3.20 mm
347 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0V-0XY ORIENTATION, 1.5mm
 V-0V-0XZ ORIENTATION, 1.5mm
 V-0V-0ZX ORIENTATION, 1.5mm
 V-0V-0XY ORIENTATION, 3.0mm
 V-0V-0XZ ORIENTATION, 3.0mm
 V-0V-0ZX ORIENTATION, 3.0mm
 
Descriptive Properties
FAA FlammabilityPASSFAR 25.853; XY ORIENTATION
OSU peak heat release rate (5 minute test)45 kW/m²FAR 25.853; XY ORIENTATION
OSU total heat release (2 minute test)44 kW-min/m²FAR 25.853; XY ORIENTATION

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80063 / 288010

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.