MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SK Chemicals ECOZEN® YF 300 Eco-friendly Bio Copolyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: ECOZEN YF 300 is eco-friendly bio copolyester which is created using natural materials based on the extract from plant or vegetable materials therefore it does not include environmental hormone bisphenol A (BPA) is a controversial never-ending human hazards. Also it is one of the excellent resins which have chemical resistance and food-stain resistance among the transparent resin used in food contact applications and its low oxygen permeability is useful for food storage container such as the airtight container.

ECOZEN YF 300 has various food contact related use of certification such as FDA (Food Contact

Notification (FCN) No. 1075), NSF (the United States), EFSA (EU), JHOSPA (Japan), NHFPC (China) and KFDA (South Korea) and it has also the certification of bioplastics such as BETA certification. ECOZEN YF 300 is obtained the GOLD Level for Cradle to Cradle (C2C) certification (the United States) and certified by the external environment-friendly products. SK Chemicals Company has obtained the GOLD Level as the world's first chemical resin supplier.

Attributes: BPA / Phthalate free. Excellent Heat Resistance. Excellent Chemical & Stain Resistance. Excellent Impact Strength. High Flexural Strength. High Transparency and Gloss. Low Processing Temperature. Less Residual Stress.

Applications: Food Container. Airtight Container. Baby Food Container. Food Bowl. Mixer & Blender. Sports Bottle, Water Bottle, Juice Bottle etc.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength at Break 44.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 51.0 MPa50 mm/min; ASTM D638
Elongation at Break 150 %50 mm/min; ASTM D638
Elongation at Yield 6.8 %50 mm/min; ASTM D638
Flexural Strength 87.0 MPa1.27 mm/min; ASTM D790
Flexural Modulus 2180 MPa1.27 mm/min; ASTM D790
Izod Impact, Notched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CASTM D648
Flammability, UL94 V-2
@Thickness 3.20 mm
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
UV Transmittance 88 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSK9938 / 291454

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.