MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Muntz metal, 60%, UNS C28000, O50 Temper, Tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Light Anneal

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Cold Worked

Common Fabrication Processes: Blanking; Forming and Bending; Hot Forging and Pressing; Hot Heading and Upsetting; Shearing

Typical uses: Architectural Panels; Decoration; Door Frames; Hardware; Large Architectural Trim; Large Sheets; Sheet; Structural, Heavy Plate; Decorative Hardware; Bolts; Brazing Rod; Condenser Plates; Condenser Tube; Evaporator Tubes; Heat Exchanger Tube; Hot Forgings; Large Nuts and Bolts; Valve Stems

Applicable Specifications: Bar – ASTM B36/B36M; Plate - ASTM B36/B36M; Seamless Condenser Tube & Ferrule Stock - Condenser Tube ASME SB111, Condenser Tube ASTM B111/B111M; Seamless Tube – ASME SB135; Sheet - ASTM B36/B36M; Strip - ASTM B36/B36M; Tube – Seamless (Metric) ASTM B135/B135M, ASTM B135, FEDERAL WW-T-791

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.39 g/cc0.303 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 8282
Hardness, Rockwell 30T 4747
Tensile Strength 386 MPa56000 psi
Tensile Strength, Yield 159 MPa23000 psi0.5% Ext
Elongation at Break 50 %50 %
Tensile Modulus 103 GPa15000 ksi
Modulus of Rigidity 38.6 GPa5600 ksi
Poissons Ratio 0.340.34Calculated
Machinability 40 %40 %
Forgeability 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000610 ohm-cm0.00000610 ohm-cm28% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.9 µm/m-°C
@Temperature 20.0 - 300 °C
11.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 10.2 W/m-K71.0 BTU-in/hr-ft²-°F
Melting Point 899 - 904 °C1650 - 1660 °F
Solidus 899 °C1650 °F
Liquidus 904 °C1660 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 621 - 788 °C1150 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 63 %59 - 63 %
Iron, Fe <= 0.070 %<= 0.070 %
Lead, Pb <= 0.090 %<= 0.090 %
Zinc, Zn 36.8 - 41 %36.8 - 41 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC28000x4 / 292906

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.