MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRICOMP™ Compound WAL34 Polybutylene Terephthalate (PBT) (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP LUBRICOMP WAL34 compound is based on Polybutylene Terephthalate (PBT) resin containing 15% PTFE, 20% aramid fiber. Added features of this grade include: Internally Lubricated, Wear Resistant.

Features: Internally Lubricated,Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Moisture Absorption 0.0500 %0.0500 %Injection Molding
 0.0900 %0.0900 %23°C/50% RH/24 hrs; ASTM D570
 0.0900 %0.0900 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psi5 mm/min; ISO 527
 46.0 MPa6670 psi5 mm/min; ASTM D638
Tensile Strength, Yield 44.0 MPa6380 psi5 mm/min; ISO 527
 46.0 MPa6670 psi5 mm/min; ASTM D638
Elongation at Break 1.3 %1.3 %5 mm/min; ISO 527
 1.5 %1.5 %5 mm/min; ASTM D638
Elongation at Yield 1.3 %1.3 %5 mm/min; ISO 527
 1.5 %1.5 %5 mm/min; ASTM D638
Tensile Modulus 4.50 GPa653 ksi50 mm/min; ASTM D638
 4.52 GPa656 ksi1 mm/min; ISO 527
Flexural Strength 78.0 MPa11300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 78.0 MPa11300 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.10 GPa595 ksi2 mm/min; ISO 178
 4.39 GPa637 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 32.0 J23.6 ft-lbASTM D256
Izod Impact, Unnotched 1.31 J/cm2.45 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 9.00 kJ/m²4.28 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J2.21 ft-lbASTM D3763
Coefficient of Friction, Dynamic 0.240.24ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.210.21ASTM D3702 Modified: Manual
K (wear) Factor 12.1 x 10-8 mm³/N-M6.00 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 51.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
28.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 84.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 206 °C403 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 215 °C
@Thickness 6.40 mm
419 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
@Thickness 3.20 mm
356 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 245 - 255 °C473 - 491 °F
Zone 3 260 - 270 °C500 - 518 °F
Melt Temperature 240 - 265 °C464 - 509 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81074 / 289021

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.