ELEVATE® EM530AA is an 18% vinyl acetate copolymer (EVA). It is a low viscosity resin particularly suitable for hot melt adhesives. It contains a pellet handling additive commonly used in some EVA resins to improve pellet flow. The reported physical properties were measured using compression molded specimens prepared per ASTM D 1928, Procedure C at 50% relative humidity and 23°C. Information provided by Westlake Chemical. |