MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® R10002E PA66/6 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Starflam R10002E is a flame retardant PA66/6 for injection molded applications. The material is halogen free and red phosphorus free.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccDAM; ISO 1183
Water Absorption 1.6 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.8 %DAM to 50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 48.0 MPa50% RH; ISO 527-2
 82.0 MPaDAM; ISO 527-2
Elongation at Break 4.9 %DAM; ISO 527-2
 6.2 %50% RH; ISO 527-2
Tensile Modulus 2300 MPa50% RH; ISO 527-2
 4100 MPaDAM; ISO 527-2
Flexural Strength 37.0 MPa50% RH; ISO 178
 102 MPaDAM; ISO 178
Flexural Modulus 1500 MPa50% RH; ISO 178
 3600 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 2.60 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 3.20 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 3.60 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 3.60 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 3.60 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
 3.90 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched 24.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 48.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 52.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 55.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 68.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 1.90 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 2.50 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 2.60 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 3.10 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 3.60 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 4.60 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 20.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 26.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Hot Wire Ignition, HWI 15 - 30 secPLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 189 °CUnannealed; 50% RH; ISO 75-2/B
 189 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 65.0 °C
@Thickness 0.400 mm
UL 746
 120 °C
@Thickness 0.800 mm
UL 746
 120 °C
@Thickness 1.60 mm
UL 746
 120 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.400 mm
UL 746
 65.0 °C
@Thickness 0.800 mm
UL 746
 75.0 °C
@Thickness 1.60 mm
UL 746
 75.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.400 mm
UL 746
 85.0 °C
@Thickness 0.800 mm
UL 746
 85.0 °C
@Thickness 1.60 mm
UL 746
 85.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.400 mm
 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 270 °CInjection
Middle Barrel Temperature 265 - 280 °CInjection
Front Barrel Temperature 270 - 280 °CInjection
Melt Temperature 265 - 280 °CInjection
Mold Temperature 60.0 - 90.0 °CInjection
Drying Temperature 75.0 - 85.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesBromine Free
 Flame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9126 / 287577

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.