MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® B 50H1 NATURAL L Nylon 66/6, Heat Stabilized, Flame Retardant, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Product Description: Ultramid® B 50H1 NATURAL L is an unreinforced copolyamide 6.6/6 based on a non-phosphorous and non-halogenated flame retardant system, heat stabilized for injection molding. This flame retardant grade, UL94 V0 at 0.4mm, offers excellent filling quality together with good stiffness. European Railways Certifications – EN 45545-2 HL2; European Railways Certifications – EN 45545-2 HL3

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Additive: Flame Retardant; Heat Stabilizer

Features: Good Mold Release; Good Stiffness; Halogen Free; Low (to None) Phosphorus Content

Use: Connectors; Electrical/Electronic Applications

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66/6-FR(30)

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183
Water Absorption 3.1 %Equilibrium, 50% RH; ISO 62
 1.1 %
@Time 86400 sec
ISO 62
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0090 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10200 psiISO 527-2
Tensile Strength, Yield 11600 psiISO 527-2
 12300 psiASTM D638
Elongation at Break 12 %ISO 527-2
 15 %ASTM D638
Elongation at Yield 4.0 %ISO 527-2
Tensile Modulus 544000 psiISO 527-1
Flexural Strength 18100 psiASTM D790
 18900 psiISO 178
Flexural Modulus 537000 psiISO 178
 551000 psiASTM D790
Izod Impact, Notched (ISO) 0.940 ft-lb/in²ASTM D256
 2.40 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 33.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
 98.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.40 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 1.70 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 3.6
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 840 V/mil
@Thickness 0.800 mm
IEC 60243-1
Dissipation Factor 0.020
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 468 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 185 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.787 mm
 V-0
@Thickness 3.30 mm
Glow Wire Ignition Temperature 1200 °F
@Thickness 1.52 mm
IEC60695-2-13
 1380 °F
@Thickness 0.787 mm
IEC60695-2-13
Glow Wire Flammability Index 1760 °F
@Thickness 0.787 mm
IEC 60695-2-12
 1760 °F
@Thickness 1.52 mm
IEC 60695-2-12
 1760 °F
@Thickness 3.30 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 473 - 482 °F
Middle Barrel Temperature 482 - 491 °F
Front Barrel Temperature 482 - 500 °F
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F
 
Descriptive Properties
European Railways CertificationsHL2EN 45545-2
 HL3EN 45545-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2069 / 310762

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.