MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Epoxies, Etc 10-3005 NS Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: These high bond strength adhesives are clear 100% solids, two component, non-sag adhesives with a quick setting time of 5-46 minutes at room temperature. They are excellent for bonding plated metals, pewter, glass, wood, ceramic, felt, cement, gem stones, most plastics and rubbers, etc. These adhesives were tested in our laboratory for flame retardancy properties. According to our test results they meet the requirements of UL94HB.

Applications: These unique adhesives are ideally suited for a wide range of electronic, electrical, industrial, structural, and jewelry applications. These adhesives are also an excellent choice for field repairs. They are offered in the popular TriggerBond® dual barrel cartridge dispensing system and bulk packaging.

Features:

  • Non-sag consistency
  • High bond strength
  • Fast room temperature cure – three speeds to choose from
  • Water & chemical resistance
  • Outstanding thermal shock resistance
  • 1:1 mix ratio
  • Impact resistance

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Compressive Modulus 8500 psi
Shear Strength 250 psiPolycarbonate
 335 psiPVC
 500 psiABS
 725 psiBrass
 750 psiStainless Steel
 900 psiGalvanized Steel
 960 psiCopper
 1000 psiCold rolled steel
 1500 psiAluminum (etched)
Izod Impact, Notched 2.70 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm
Dielectric Constant 4.0
@Frequency 1000 Hz
Dielectric Strength 420 V/mil
Dissipation Factor 0.017
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 - 20.0 min
 24.0 - 48.0 hourHandling time
 
Descriptive Properties
ColorSemi-transparent (available in black)
Mix Ratio1:1by volume
Working Time3-5 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX074 / 316751

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.