MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inov Chem Donfoam 812PIR HCFC-141B Base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonFoam 812/PIR is a kind of blend polyols with hcfc-141b foaming agent, with polyol as the main raw material, mixed with special auxiliary agent, suitable for the insulation of construction, transportation, shell and other products. The polyurethane product prepared by reacting it with isocyanate has the following advantages:
1.Foam has uniform strength and dimensional stability in all directions
2.The foam products can be cut into different shapes according to the requirements of the product
3.Excellent thermal insulation performance

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 - 1.25 g/cc
Density 0.0270 - 0.0310 g/ccFree density, High Pressure
 0.0280 - 0.0320 g/ccFree density, Manual mix
 >= 0.0500 g/ccOverall Molding Density; GB/T 6343
Viscosity 200 - 300 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.150 MPaGB/T8813
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 15.0 °C
GB/T 3399
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CRaw material temperature, Manual mix
 20.0 - 25.0 °CRaw material temperature, High pressure
Cure Time 270 - 320 secTack free time, High Pressure
 300 - 350 secTack free time, Manual mix
Gel Time 2.00 - 2.67 minHigh Pressure
 2.30 - 3.00 minManual mix
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow to brown transparent liquid
Closed-cell rate=90%GB/T 10799
Cream time25-45 secHigh Pressure
 30-50 secManual mix
Dimensional stability=0.5%24h, -20?; GB/T8811
 =1.0%24h, 100?; GB/T8811
FlammabilityB2, B1GB/T 8624
OH value150-250 mgKOH/g
Recommended Ratio100DonFoam 812/PIR
 150-200Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM029 / 312558

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.