MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ X11 ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Automotive: High heat resistance. Excellent flow/impact balance. High gloss.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 3.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 18 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength at Break 33.0 MPa5 mm/min; ASTM D638
 35.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 42.0 MPa5 mm/min; ASTM D638
 46.0 MPa50 mm/min; ISO 527
Elongation at Break 18 %50 mm/min; ISO 527
 27 %5 mm/min; ASTM D638
Elongation at Yield 2.6 %50 mm/min; ISO 527
 2.6 %5 mm/min; ASTM D638
Tensile Modulus 2350 MPa1mm/min; ISO 527
 2370 MPa5 mm/min; ASTM D638
Flexural Yield Strength 69.0 MPa2 mm/min; ISO 178
 71.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2170 MPa2 mm/min; ISO 178
 2290 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 300 J/mASTM D256
 240 J/m
@Thickness 6.40 mm
ASTM D256
Izod Impact, Notched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 25.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 86.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 93.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 104 °CRate B/50; ISO 306
 106 °CRate B/120; ISO 306
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 230 - 275 °CInjection Molding
Zone 1 195 - 210 °C
Zone 2 210 - 225 °C
Zone 3 230 - 255 °C
Melt Temperature 230 - 275 °C
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 90.0 - 95.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.10 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10117 / 243584

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.