MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Lanxess Pocan® B 1700 000000 PBT  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Extrusion Grade; Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: PBT, non-reinforced, extrusion, food contact

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Water Absorption 0.50 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 0.20 %23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number 158 cm³/gISO 307, 1157, 1628
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 260 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaISO 527-1/-2
Elongation at Break >= 50 %Nominal; ISO 527-1/-2
Elongation at Yield 4.0 %ISO 527-1/-2
Tensile Modulus 2600 MPaISO 527-1/-2
Charpy Impact Unnotched 230 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Impact 3877Puncture maximum force (N); ISO 6603-2
 3926
@Temperature -30.0 °C
Puncture maximum force (N); ISO 6603-2
Puncture Energy 23.0 JISO 6603-2
 16.0 J
@Temperature -30.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance <= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243-1
Dissipation Factor 0.0015
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°CISO 11359-1/-2
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 45.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 HB
@Thickness 0.800 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
FormPellets
ISO Short NameISO 7792-1-PBT,G,13-030
ProcessingOther extrusion
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANX0847 / 99062

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.