MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco SYMBOL 2190 Turbine Oil TEP
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Turbine Oil Symbol 2190 TEP was developed primarily as a circulating system oil for marine gear turbine sets.

Chevron Turbine Oil Symbol 2190 TEP provides mild extreme pressure protection as well as resistance to rust, oxidation, corrosion, and foaming. Chevron Turbine Oil Symbol 2190 TEP has outstanding thermal and oxidation stability which allows it to withstand the high temperatures found in turbine bearing and gear lubrication.

The foam inhibition prevents the buildup of foam in the sump tank with possible vent pipe overflow. Its excellent stability, high viscosity index, and rust and corrosion inhibition assures high film strength lubrication for gears and bearings, as well as rust and corrosion protection. Together, these qualities mean both long lubricant and equipment life.

Applications

Chevron Turbine Oil Symbol 2190 TEP is recommended for use in marine turbine reduction gears, where heavy tooth loading and shock loads are encountered. The extreme pressure properties enable Chevron Turbine Oil Symbol 2190 TEP to meet the requirements of MIL-PRF-17331J.

Do not filter through Fullers Earth-type filtration systems since this would deplete the additive package. Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Key Words: CPS Number: 253030; MSDS Number: 4764
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 31.9 °31.9 °
Viscosity Measurement 9999Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 415 SUS415 SUS
Saybolt Viscosity at 210°F 59.1 SUS59.1 SUS
Kinematic Viscosity at 40°C (104°F) 79.8 cSt79.8 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 9.7 cSt9.7 cStASTM D445
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.160.16mg KOH/g
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 246 °C475 °FASTM D92
 
Descriptive Properties
Color0.5
Conradson Carbon Residue, mass %0.1
Corrosion, Copper Strip Test 3h1
Rust preventative Test Procedure BPassSynthetic Sea Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV368 / 74983

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.