MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Erbslöh Aluminium DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Heat Treatment Condition T6 (Quench in water at RT)
  • abrasive stability
  • high stiffness (E-modulus)
  • resistance even at high temperatures
  • good grindability

PEAK DISPAL materials allow the manufacturing of pistons for highest operational demands.

Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.4605 - 2.7195 g/cc0.088891 - 0.098248 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers >= 160>= 160
Tensile Strength at Break  >= 348 MPa
@Temperature 150 °C
>= 50500 psi
@Temperature 302 °F
 >= 380 MPa
@Temperature 20.0 °C
>= 55100 psi
@Temperature 68.0 °F
Tensile Strength, Yield  >= 310 MPa
@Temperature 150 °C
>= 45000 psi
@Temperature 302 °F
 >= 350 MPa
@Temperature 20.0 °C
>= 50800 psi
@Temperature 68.0 °F
Elongation at Break  >= 0.40 %
@Temperature 20.0 °C
>= 0.40 %
@Temperature 68.0 °F
 >= 0.70 %
@Temperature 150 °C
>= 0.70 %
@Temperature 302 °F
Modulus of Elasticity  >= 81.0 GPa
@Temperature 150 °C
>= 11700 ksi
@Temperature 302 °F
 >= 88.0 GPa
@Temperature 20.0 °C
>= 12800 ksi
@Temperature 68.0 °F
Poissons Ratio  0.297
@Temperature 20.0 °C
0.297
@Temperature 68.0 °F
 0.297
@Temperature 100 °C
0.297
@Temperature 212 °F
 0.299
@Temperature 150 °C
0.299
@Temperature 302 °F
 0.302
@Temperature 200 °C
0.302
@Temperature 392 °F
 0.302
@Temperature 250 °C
0.302
@Temperature 482 °F
 0.305
@Temperature 300 °C
0.305
@Temperature 572 °F
Shear Modulus  32.0 GPa
@Temperature 300 °C
4640 ksi
@Temperature 572 °F
 33.0 GPa
@Temperature 250 °C
4790 ksi
@Temperature 482 °F
 34.0 GPa
@Temperature 150 °C
4930 ksi
@Temperature 302 °F
 34.0 GPa
@Temperature 200 °C
4930 ksi
@Temperature 392 °F
 35.0 GPa
@Temperature 100 °C
5080 ksi
@Temperature 212 °F
 36.0 GPa
@Temperature 20.0 °C
5220 ksi
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 - 0.00000700 ohm-cm0.00000660 - 0.00000700 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.4 - 16.4 µm/m-°C
@Temperature 20.0 - 100 °C
8.56 - 9.11 µin/in-°F
@Temperature 68.0 - 212 °F
 15.6 - 16.6 µm/m-°C
@Temperature 20.0 - 200 °C
8.67 - 9.22 µin/in-°F
@Temperature 68.0 - 392 °F
 16.3 - 17.3 µm/m-°C
@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.860 - 0.900 J/g-°C0.206 - 0.215 BTU/lb-°F
Thermal Conductivity  118.9 W/m-K
@Temperature 400 °C
825.2 BTU-in/hr-ft²-°F
@Temperature 752 °F
 123.6 W/m-K
@Temperature 200 °C
857.8 BTU-in/hr-ft²-°F
@Temperature 392 °F
 123.8 W/m-K
@Temperature 300 °C
859.2 BTU-in/hr-ft²-°F
@Temperature 572 °F
 126.5 W/m-K
@Temperature 100 °C
877.9 BTU-in/hr-ft²-°F
@Temperature 212 °F
 131.6 W/m-K
@Temperature 30.0 °C
913.3 BTU-in/hr-ft²-°F
@Temperature 86.0 °F
Melting Point 537 - 833 °C999 - 1530 °F
Solidus 537.1 - 543.1 °C998.8 - 1010 °F
Liquidus 826.5 - 832.5 °C1520 - 1531 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 68 %68 %As Balance
Copper, Cu 1.0 %1.0 %
Magnesium, Mg 1.0 %1.0 %
Silicon, Si 30 %30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Erbslöh Aluminium DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Erbslöh Aluminium DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Erbslöh Aluminium DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition F

NPEAK03 / 101608

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.