MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NRI Trans-Wrap Carbon Fiber Epoxy Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Trans-Wrap™ is a bidirectional non-woven 100% carbon fiber composite, saturated with NRI’s proprietary epoxy system, Thermo-Poxy™. The Trans-Wrap carbon fiber is oriented in the 0° / 90° directions and is stitched resulting in outstanding tensile values in both directions. It has a high thickness per layer resulting in fewer layers needed for reinforcement and quicker applications. The Thermo-Poxy Epoxy system is a two-part, 100% solid epoxy designed for use in a wide variety of environments possessing excellent chemical resistance and high temperature ratings.

Typical Applications:

  • Pipeline Repair
  • Containment and shear reinforcement
  • Bridge column repair
  • Pile repair
Benefits:
  • Long working time even in hot environments
  • High temperature rating with an ambient cured epoxy
  • Thick laminate for cost effective installation
  • Applicable in damp and wet environments
  • High strength and light weight
  • Manufactured in ISO 9001 certified facility
  • Full factory engineering calculations, consultation, and support ensuring safe and successful repairs

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Tensile Strength 896 MPa130000 psiAxial; ASTM D3039
 2960 MPa429000 psiHoop; ASTM D3039
Elongation at Break 1.46 %1.46 %ASTM D3039
Tensile Modulus 49.3 GPa7150 ksiASTM D3039
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -45.0 °C-49.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min
@Temperature 24.0 °C
4.00 hour
@Temperature 75.2 °F
Set Time
Pot Life 75.0 min75.0 min
Working Life 45.0 min
@Temperature 24.0 °C
45.0 min
@Temperature 75.2 °F
Gel Time 161 min
@Temperature 24.0 °C
161 min
@Temperature 75.2 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber
Hexcel® HexTow® AS4D Carbon Fiber - Epoxy Composite
Overview of materials for Epoxy/Carbon Fiber Composite
DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors
NRI Thermo-Wrap™ CF Carbon Fiber Composite

PNRI028 / 192044

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.