MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Novatec Novablend® 5021 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: Novablend® 5021 is a general purpose, rigid, PVC extrusion profile compound in pellet form. The formulation is designed to provide good processing characteristics, with excellent transparency and gloss. Raw material appearance is Clear Pellets.

Applications: Novablend® 5021 is used for clear extrusions where transparency is important.

Information supplied by the manufacturer.

PolyOne (Avient) acquired the Novatec polymer resin product line. This grade is not a part of their current product line

Key Words: Good processing characteristics, with excellent transparency and gloss
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.34 g/cc0.0470 - 0.0484 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.4 MPa6000 psiASTM D638
Modulus of Elasticity 2.76 GPa400 ksiASTM D638
Flexural Yield Strength 77.2 MPa11200 psiASTM D790
Flexural Modulus 2.55 GPa370 ksiASTM D790
Izod Impact, Notched 8.00 J/cm15.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
European Beech Wood
ChevronTexaco ATF+3® Automatic Transmission Fluid
Aurora Plastics TufTech™ GA-8705-03 Natural Gloss PVC Compound
Sylvin Technologies 8960-60 Natural PVC Extrusion Compound
Solvay Chemicals NOCOLOK® Thickener (water soluble)

PNV040 / 55487

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.